    Hi, The lead just melts right away, and we had to keep the kiln turning every two or three mins. as not to warp the kiln because if any longer the hot lime just sitting there would warp the kiln! By turning the kiln also would drive the lime could work forward and drop into the drag chain conveyer trench to the hot lime tank! The lead just goes into the dissolving tank along with the hot lime from the hot lime tank for settling out after that any lead or anything not usable for the making whit liquor for cooking the wood chips was slaked out and went to a deposit area!

  2. The Following User Says Thank You to skibo For This Useful Post:

    PJs (Jan 10, 2019)

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •